Allgemein
Property | Value | Shape | Related Standards |
---|---|---|---|
Dichte | 4.65 g/cm³ Show Material materials with Dichte of 4.65 g/cm³ | Bar, Billet | |
4.65 g/cm³ Show Material materials with Dichte of 4.65 g/cm³ | AMS 4981B, MIL-T 9047G |
Abmessung
Property | Temperature | Value | Shape | Comment |
---|---|---|---|---|
Dimensions | 15-65 mm diameter up to 6000 mm length °C | 7-14.5 mm diameter up to 3000 mm length | Bar | |
Durchmesser | 7 mm Show Material materials with Durchmesser of 7 mm | Bar | ||
115 mm Show Material materials with Durchmesser of 115 mm | Bar | |||
130 mm Show Material materials with Durchmesser of 130 mm | Billet | |||
350 mm Show Material materials with Durchmesser of 350 mm | Billet | |||
Länge | 3000 mm Show Material materials with Länge of 3000 mm | Billet | ||
4500 mm Show Material materials with Länge of 4500 mm | Billet | |||
6000 mm Show Material materials with Länge of 6000 mm | Bar | max |
Mechanisch
Property | Value | Shape | Related Standards |
---|---|---|---|
Dehnung | 13.0 % Show Material materials with Dehnung of 13.0 % | Bar, Billet | |
Elastizitätsmodul | 114.0 GPa Show Material materials with Elastizitätsmodul of 114.0 GPa | Bar, Billet | |
114 GPa Show Material materials with Elastizitätsmodul of 114 GPa | AMS 4981B, MIL-T 9047G | ||
Härte, Brinell | 360.0 Show Material materials with Härte, Brinell of 360.0 | Bar, Billet | |
Härte, Rockwell C | 39.0 [-] Show Material materials with Härte, Rockwell C of 39.0 [-] | Bar, Billet | |
Härte, Vickers | 376.0 Show Material materials with Härte, Vickers of 376.0 | Bar, Billet | |
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Bar, Billet | |
Schubmodule | 42.9 GPa Show Material materials with Schubmodule of 42.9 GPa | Bar, Billet | |
Streckgrenze | 1103.0 MPa Show Material materials with Streckgrenze of 1103.0 MPa | AMS 4981B, MIL-T 9047G | |
1120.0 MPa Show Material materials with Streckgrenze of 1120.0 MPa | Bar, Billet | ||
Zugfestigkeit | 1172.0 MPa Show Material materials with Zugfestigkeit of 1172.0 MPa | AMS 4981B, MIL-T 9047G | |
1210.0 MPa Show Material materials with Zugfestigkeit of 1210.0 MPa | Bar, Billet |
Thermisch
Property | Temperature | Value | Related Standards | Shape |
---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20 °C | 0.0000094 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.0000094 1/K | AMS 4981B, MIL-T 9047G | |
20 °C | 0.0000103 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.0000103 1/K | AMS 4981B, MIL-T 9047G | ||
20 °C | 0.0000104 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.0000104 1/K | AMS 4981B, MIL-T 9047G | ||
100 °C | 0.0000094 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.0000094 1/K | AMS 4981B, MIL-T 9047G | ||
315 °C | 0.0000103 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.0000103 1/K | AMS 4981B, MIL-T 9047G | ||
538 °C | 0.0000104 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.0000104 1/K | AMS 4981B, MIL-T 9047G | ||
Schmelzpunkt | 1593.0 °C Show Material materials with Schmelzpunkt of 1593.0 °C | AMS 4981B, MIL-T 9047G | ||
1595.0 - 1675.0 °C Show Material materials with Schmelzpunkt of 1595.0 - 1675.0 °C | Bar, Billet | |||
Spezifische Wärmekapazität | 500 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 500 J/(kg·K) | AMS 4981B, MIL-T 9047G | ||
Wärmeleitfähigkeit | 7.7 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 7.7 W/(m·K) | AMS 4981B, MIL-T 9047G | Bar, Billet |
Elektrisch
Property | Value | Related Standards |
---|---|---|
spezifischer Widerstand | 2e-06 Ω·m Show Material materials with spezifischer Widerstand of 2e-06 Ω·m | AMS 4981B, MIL-T 9047G |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminium | 5.5 - 6.5 % Show Material materials with Aluminium of 5.5 - 6.5 % | AMS 4981B, MIL-T 9047G | |
6.0 % Show Material materials with Aluminium of 6.0 % | Bar, Billet | ||
Eisen | 0.15 Show Material materials with Eisen of 0.15 | AMS 4981B, MIL-T 9047G | |
Kohlenstoff | 0.04 Show Material materials with Kohlenstoff of 0.04 | AMS 4981B, MIL-T 9047G | |
Molybdän | 5.5 - 6.5 % Show Material materials with Molybdän of 5.5 - 6.5 % | AMS 4981B, MIL-T 9047G | |
6.0 % Show Material materials with Molybdän of 6.0 % | Bar, Billet | ||
Sauerstoff | 0.5 Show Material materials with Sauerstoff of 0.5 | AMS 4981B, MIL-T 9047G | |
Stickstoff | 0.04 Show Material materials with Stickstoff of 0.04 | AMS 4981B, MIL-T 9047G | |
Wasserstoff | 0.0125 Show Material materials with Wasserstoff of 0.0125 | AMS 4981B, MIL-T 9047G | |
Zinn | 1.75 - 2.25 % Show Material materials with Zinn of 1.75 - 2.25 % | AMS 4981B, MIL-T 9047G | |
2.0 % Show Material materials with Zinn of 2.0 % | Bar, Billet | ||
Zirkonium | 3.5 - 4.5 % Show Material materials with Zirkonium of 3.5 - 4.5 % | AMS 4981B, MIL-T 9047G | |
4.0 % Show Material materials with Zirkonium of 4.0 % | Bar, Billet |