Allgemein
Property | Value | Shape |
---|---|---|
Dichte | 4.49 g/cm³ Show Material materials with Dichte of 4.49 g/cm³ | Tube |
Abmessung
Property | Value | Shape |
---|---|---|
Durchmesser | 5 mm Show Material materials with Durchmesser of 5 mm | Tube |
25.4 mm Show Material materials with Durchmesser of 25.4 mm | Billet | |
125 mm Show Material materials with Durchmesser of 125 mm | Billet | |
130 mm Show Material materials with Durchmesser of 130 mm | Tube | |
Länge | 1000 mm Show Material materials with Länge of 1000 mm | Tube |
5000 mm Show Material materials with Länge of 5000 mm | Tube | |
Wall thickness | 0.5 - 9.0 mm Show Material materials with Wall thickness of 0.5 - 9.0 mm | Tube |
2.5 - 21.0 mm Show Material materials with Wall thickness of 2.5 - 21.0 mm | Billet |
Mechanisch
Property | Value | Shape | Comment |
---|---|---|---|
Dehnung | 15.0 - 25.0 % Show Material materials with Dehnung of 15.0 - 25.0 % | Tube | |
Elastizitätsmodul | 100.0 - 120.0 GPa Show Material materials with Elastizitätsmodul of 100.0 - 120.0 GPa | Typical for Low Alloy Titanium | |
Zugfestigkeit | 480.0 - 680.0 MPa Show Material materials with Zugfestigkeit of 480.0 - 680.0 MPa | Tube |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 7.599999999999997e-06 - 9.9e-06 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 7.599999999999997e-06 - 9.9e-06 1/K | Typical for Low Alloy Titanium |
Schmelzpunkt | 1650.0 - 1705.0 °C Show Material materials with Schmelzpunkt of 1650.0 - 1705.0 °C | Typical for Low Alloy Titanium |
Spezifische Wärmekapazität | 515.0 - 597.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 515.0 - 597.0 J/(kg·K) | Typical for Low Alloy Titanium |
Wärmeleitfähigkeit | 15.0 - 22.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 15.0 - 22.0 W/(m·K) | Typical for Low Alloy Titanium |
Chemical properties
Property | Value | Shape |
---|---|---|
Aluminium | 0.2 - 0.7 % Show Material materials with Aluminium of 0.2 - 0.7 % | Billet, Tube |
Kohlenstoff | 0.07 Show Material materials with Kohlenstoff of 0.07 | Billet, Tube |
Sauerstoff | 0.12 Show Material materials with Sauerstoff of 0.12 | Billet, Tube |
Silizium | 0.1 Show Material materials with Silizium of 0.1 | Billet, Tube |
Stickstoff | 0.04 Show Material materials with Stickstoff of 0.04 | Billet, Tube |
Zirkonium | 0.3 Show Material materials with Zirkonium of 0.3 | Billet, Tube |