Allgemein
Property | Value | Related Standards | Shape |
---|---|---|---|
Dichte | 4.51 g/cm³ Show Material materials with Dichte of 4.51 g/cm³ | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
Abmessung
Property | Value | Related Standards | Shape |
---|---|---|---|
Durchmesser | 25.4 mm Show Material materials with Durchmesser of 25.4 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
125 mm Show Material materials with Durchmesser of 125 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet | |
Wall thickness | 2.5 - 21.0 mm Show Material materials with Wall thickness of 2.5 - 21.0 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
Mechanisch
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Dehnung | 10.0 - 30.0 % Show Material materials with Dehnung of 10.0 - 30.0 % | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet | |
Elastizitätsmodul | 100.0 - 120.0 GPa Show Material materials with Elastizitätsmodul of 100.0 - 120.0 GPa | Typical for Titanium Alpha Alloy | ||
Zugfestigkeit | 440.0 - 637.0 MPa Show Material materials with Zugfestigkeit of 440.0 - 637.0 MPa | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 7.599999999999997e-06 - 1.1e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 7.599999999999997e-06 - 1.1e-05 1/K | Typical for Titanium Alpha Alloy |
Schmelzpunkt | 1540.0 - 1715.0 °C Show Material materials with Schmelzpunkt of 1540.0 - 1715.0 °C | Typical for Titanium Alpha Alloy |
Spezifische Wärmekapazität | 460.0 - 527.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460.0 - 527.0 J/(kg·K) | Typical for Titanium Alpha Alloy |
Wärmeleitfähigkeit | 4.0 - 17.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 4.0 - 17.0 W/(m·K) | Typical for Titanium Alpha Alloy |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminium | 0.4 - 1.4 % Show Material materials with Aluminium of 0.4 - 1.4 % | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
Eisen | 0.3 Show Material materials with Eisen of 0.3 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
Kohlenstoff | 0.1 Show Material materials with Kohlenstoff of 0.1 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
Mangan | 0.5 - 1.3 % Show Material materials with Mangan of 0.5 - 1.3 % | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
Sauerstoff | 0.15 Show Material materials with Sauerstoff of 0.15 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
Silizium | 0.12 Show Material materials with Silizium of 0.12 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
Stickstoff | 0.05 Show Material materials with Stickstoff of 0.05 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
Wasserstoff | 0.012 Show Material materials with Wasserstoff of 0.012 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
Zirkonium | 0.3 Show Material materials with Zirkonium of 0.3 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |