Allgemein
Property | Value | Related Standards | Shape |
---|---|---|---|
Dichte | 4.505 g/cm³ Show Material materials with Dichte of 4.505 g/cm³ | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
Abmessung
Property | Value | Related Standards | Shape |
---|---|---|---|
Durchmesser | 5 mm Show Material materials with Durchmesser of 5 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Tube |
25.4 mm Show Material materials with Durchmesser of 25.4 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet | |
125 mm Show Material materials with Durchmesser of 125 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet | |
130 mm Show Material materials with Durchmesser of 130 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Tube | |
Länge | 1000 mm Show Material materials with Länge of 1000 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Tube |
5000 mm Show Material materials with Länge of 5000 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Tube | |
Wall thickness | 0.5 - 9.0 mm Show Material materials with Wall thickness of 0.5 - 9.0 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Tube |
2.5 - 21.0 mm Show Material materials with Wall thickness of 2.5 - 21.0 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
Mechanisch
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Dehnung | 11.0 - 30.0 % Show Material materials with Dehnung of 11.0 - 30.0 % | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet | |
Elastizitätsmodul | 120.0 GPa Show Material materials with Elastizitätsmodul of 120.0 GPa | Typical for Pure Titanium | ||
Poissonzahl | 0.361 [-] Show Material materials with Poissonzahl of 0.361 [-] | Typical for Pure Titanium | ||
Schubmodule | 46.0 GPa Show Material materials with Schubmodule of 46.0 GPa | Typical for Pure Titanium | ||
Zugfestigkeit | 265.0 - 490.0 MPa Show Material materials with Zugfestigkeit of 265.0 - 490.0 MPa | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
Thermisch
Property | Temperature | Value | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 8.400000000000001e-06 - 8.599999999999999e-06 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 8.400000000000001e-06 - 8.599999999999999e-06 1/K | Typical for Pure Titanium | |||
Schmelzpunkt | 1670.0 °C Show Material materials with Schmelzpunkt of 1670.0 °C | Typical for Pure Titanium | |||
Spezifische Wärmekapazität | 100 °C | 540 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 540 J/(kg·K) | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube | |
Wärmeleitfähigkeit | 18.85 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 18.85 W/(m·K) | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Eisen | 0.15 Show Material materials with Eisen of 0.15 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube |
Kohlenstoff | 0.05 Show Material materials with Kohlenstoff of 0.05 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube |
Sauerstoff | 0.1 Show Material materials with Sauerstoff of 0.1 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube |
Silizium | 0.08 Show Material materials with Silizium of 0.08 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube |
Stickstoff | 0.04 Show Material materials with Stickstoff of 0.04 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube |
Wasserstoff | 0.008 Show Material materials with Wasserstoff of 0.008 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube |