Allgemein
Property | Value |
---|---|
Dichte | 2.71 g/cm³ Show Material materials with Dichte of 2.71 g/cm³ |
Mechanisch
Property | Temperature | Value | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Dehnung | 20.0 °C | 2.0 % Show Material materials with Dehnung of 2.0 % | EN 573-3 | Plate | A50 |
20.0 °C | 3.0 % Show Material materials with Dehnung of 3.0 % | EN 573-3 | Plate | A50 | |
20.0 °C | 4.0 % Show Material materials with Dehnung of 4.0 % | EN 573-3 | Plate | A50 | |
20.0 °C | 5.0 % Show Material materials with Dehnung of 5.0 % | EN 573-3 | Plate | A50 | |
20.0 °C | 8.0 % Show Material materials with Dehnung of 8.0 % | EN 573-3 | Plate | ||
Elastizitätsmodul | 67.0 GPa Show Material materials with Elastizitätsmodul of 67.0 GPa | ||||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 1000 Series Aluminium | |||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 1000 Series Aluminium | |||
Schubmodule | 25.9 GPa Show Material materials with Schubmodule of 25.9 GPa | Typical for Wrought 1000 Series Aluminium | |||
Streckgrenze | 40.0 MPa Show Material materials with Streckgrenze of 40.0 MPa | ||||
20.0 °C | 75.0 MPa Show Material materials with Streckgrenze of 75.0 MPa | EN 573-3 | Plate | RP02 | |
Zugfestigkeit | 80.0 MPa Show Material materials with Zugfestigkeit of 80.0 MPa | ||||
20.0 °C | 105.0 - 145.0 MPa Show Material materials with Zugfestigkeit of 105.0 - 145.0 MPa | EN 573-3 | Plate |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 2.35e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.35e-05 1/K | |
Schmelzpunkt | 645.0 - 660.0 °C Show Material materials with Schmelzpunkt of 645.0 - 660.0 °C | Typical for Wrought 1000 Series Aluminium |
Spezifische Wärmekapazität | 897.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 897.0 J/(kg·K) | |
Wärmeleitfähigkeit | 221.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 221.0 W/(m·K) |
Elektrisch
Property | Value | Comment |
---|---|---|
Elektrische Leitfähigkeit | 33000000.0 - 38000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 33000000.0 - 38000000.0 S/m | Typical for Wrought 1000 Series Aluminium |
spezifischer Widerstand | 2.7e-08 - 3e-08 Ω·m Show Material materials with spezifischer Widerstand of 2.7e-08 - 3e-08 Ω·m | Typical for Wrought 1000 Series Aluminium |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Bor | 0.05 Show Material materials with Bor of 0.05 | EN 573-3 | |
Chrom | 0.01 Show Material materials with Chrom of 0.01 | EN 573-3 | |
Eisen | 0.4 Show Material materials with Eisen of 0.4 | EN 573-3 | Plate |
Gallium | 0.03 Show Material materials with Gallium of 0.03 | EN 573-3 | |
Kupfer | 0.02 Show Material materials with Kupfer of 0.02 | EN 573-3 | |
0.05 Show Material materials with Kupfer of 0.05 | EN 573-3 | Plate | |
Magnesium | 0.05 Show Material materials with Magnesium of 0.05 | EN 573-3 | Plate |
Mangan | 0.01 Show Material materials with Mangan of 0.01 | EN 573-3 | |
0.05 Show Material materials with Mangan of 0.05 | EN 573-3 | Plate | |
Silizium | 0.1 Show Material materials with Silizium of 0.1 | EN 573-3 | |
0.25 Show Material materials with Silizium of 0.25 | EN 573-3 | Plate | |
Titan | 0.05 % Show Material materials with Titan of 0.05 % | EN 573-3 | Plate |
0.1 - 0.2 % Show Material materials with Titan of 0.1 - 0.2 % | EN 573-3 | ||
Zink | 0.05 Show Material materials with Zink of 0.05 | EN 573-3 | |
0.07 Show Material materials with Zink of 0.07 | EN 573-3 | Plate |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent | |
Workability | Excellent workability. |