Allgemein
Property | Value | Related Standards | Shape |
---|---|---|---|
Dichte | 2.68 g/cm³ Show Material materials with Dichte of 2.68 g/cm³ | EN 573-3 | Strip, Sheet, Plate |
2.68 g/cm³ Show Material materials with Dichte of 2.68 g/cm³ |
Mechanisch
Property | Value | Comment |
---|---|---|
Elastizitätsmodul | 69.0 GPa Show Material materials with Elastizitätsmodul of 69.0 GPa | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 4000 Series Aluminium |
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 4000 Series Aluminium |
Schubmodule | 26.0 GPa Show Material materials with Schubmodule of 26.0 GPa | Typical for Wrought 4000 Series Aluminium |
Streckgrenze | 70.0 MPa Show Material materials with Streckgrenze of 70.0 MPa | |
Zugfestigkeit | 110.0 MPa Show Material materials with Zugfestigkeit of 110.0 MPa |
Thermisch
Property | Temperature | Value | Related Standards | Shape |
---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 2.1600000000000003e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.1600000000000003e-05 1/K | |||
20 °C | 2.16e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.16e-05 1/K | EN 573-3 | Strip, Sheet, Plate | |
100 °C | 2.16e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.16e-05 1/K | EN 573-3 | Strip, Sheet, Plate | |
Schmelzpunkt | 575.0 - 615.0 °C Show Material materials with Schmelzpunkt of 575.0 - 615.0 °C | EN 573-3 | Strip, Sheet, Plate | |
Spezifische Wärmekapazität | 890.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 890.0 J/(kg·K) | |||
Wärmeleitfähigkeit | 180 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 180 W/(m·K) | EN 573-3 | Strip, Sheet, Plate | |
180.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 180.0 W/(m·K) |
Elektrisch
Property | Value | Related Standards | Shape |
---|---|---|---|
Elektrische Leitfähigkeit | 27000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 27000000.0 S/m | EN 573-3 | Strip, Sheet, Plate |
spezifischer Widerstand | 3.7e-08 Ω·m Show Material materials with spezifischer Widerstand of 3.7e-08 Ω·m | EN 573-3 | Strip, Sheet, Plate |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Eisen | 0.8 % Show Material materials with Eisen of 0.8 % | EN 573-3 | |
0.80 % Show Material materials with Eisen of 0.80 % | EN 573-3 | Strip, Sheet, Plate | |
Kupfer | 0.25 % Show Material materials with Kupfer of 0.25 % | EN 573-3 | Strip, Sheet, Plate |
Mangan | 0.1 % Show Material materials with Mangan of 0.1 % | EN 573-3 | Strip, Sheet, Plate |
Silizium | 6.8 - 8.2 % Show Material materials with Silizium of 6.8 - 8.2 % | EN 573-3 | Strip, Sheet, Plate |
Zink | 0.2 % Show Material materials with Zink of 0.2 % | EN 573-3 | Strip, Sheet, Plate |
Technological properties
Property | ||
---|---|---|
Workability | Moderate Workability |