Allgemein
Property | Value |
---|---|
Dichte | 0.905 - 0.915 g/cm³ Show Material materials with Dichte of 0.905 - 0.915 g/cm³ |
Mechanisch
Property | Value |
---|---|
Dehnung | 200.0 - 900.0 % Show Material materials with Dehnung of 200.0 - 900.0 % |
Zugfestigkeit | 4.0 - 8.0 MPa Show Material materials with Zugfestigkeit of 4.0 - 8.0 MPa |
Thermisch
Property | Value |
---|---|
Schmelzpunkt | 102.0 - 122.0 °C Show Material materials with Schmelzpunkt of 102.0 - 122.0 °C |
Elektrisch
Property | Value |
---|---|
spezifischer Widerstand | 1000000000000000 Ω·m Show Material materials with spezifischer Widerstand of 1000000000000000 Ω·m |
Optisch
Property | Value |
---|---|
Transparenz | yes |
Technological properties
Property | ||
---|---|---|
Application areas | stretch films, frozen food bags, medical packaging | |
Processing methods | injection molding, extrusion, blow molding, casting |