Allgemein
Property | Value |
---|---|
Dichte | 0.95 - 1.33 g/cm³ Show Material materials with Dichte of 0.95 - 1.33 g/cm³ |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 100.0 - 700.0 % Show Material materials with Dehnung of 100.0 - 700.0 % | |
Zugfestigkeit | 7.0 - 38.0 MPa Show Material materials with Zugfestigkeit of 7.0 - 38.0 MPa | at 100-700% strain |
Thermisch
Property | Value |
---|---|
Koeffizient der thermischen Ausdehnung | 0.000195 - 0.00026 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.000195 - 0.00026 1/K |
Optisch
Property | Value |
---|---|
Transparenz | no |
Technological properties
Property | ||
---|---|---|
Application areas | Oil production equipment, fuel hoses, in-tank insulators, refrigerant hoses, O-rings | |
Processing methods | Compression molding, extrusion, vulcanization |