Allgemein
Property | Value |
---|---|
Dichte | 1.42 - 1.47 g/cm³ Show Material materials with Dichte of 1.42 - 1.47 g/cm³ |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 1.5 % Show Material materials with Dehnung of 1.5 % | |
Elastizitätsmodul | 100.0 - 125.0 GPa Show Material materials with Elastizitätsmodul of 100.0 - 125.0 GPa | |
Zugfestigkeit | 1800.0 - 2000.0 MPa Show Material materials with Zugfestigkeit of 1800.0 - 2000.0 MPa | at 1.5% strain |
Thermisch
Property | Value |
---|---|
Schmelzpunkt | 220 °C Show Material materials with Schmelzpunkt of 220 °C |
Optisch
Property | Value |
---|---|
Transparenz | no |
Technological properties
Property | ||
---|---|---|
Application areas | Lightweight car body, structural components, sporting goods, under hood applications, housings | |
Fillers | 60% Carbon Fiber | |
Processing methods | Thermoforming, back injection molding, insert moulding |