Allgemein
Property | Value |
---|---|
Dichte | 1.72 - 1.79 g/cm³ Show Material materials with Dichte of 1.72 - 1.79 g/cm³ |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 2.4 % Show Material materials with Dehnung of 2.4 % | |
Elastizitätsmodul | 30.0 - 46.0 GPa Show Material materials with Elastizitätsmodul of 30.0 - 46.0 GPa | |
Zugfestigkeit | 730.0 - 1050.0 MPa Show Material materials with Zugfestigkeit of 730.0 - 1050.0 MPa | at 2.4% strain |
Thermisch
Property | Value |
---|---|
Schmelzpunkt | 220 °C Show Material materials with Schmelzpunkt of 220 °C |
Optisch
Property | Value |
---|---|
Transparenz | no |
Technological properties
Property | ||
---|---|---|
Application areas | Lightweight car body, under hood applications, sporting goods, car structure | |
Fillers | 60% Glass Fiber | |
Processing methods | Thermoforming, back injection molding, insert moulding |