Allgemein
Property | Value |
---|---|
Dichte | 1.750 g/cm³ Show Material materials with Dichte of 1.750 g/cm³ |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 2.4 - 2.6 % Show Material materials with Dehnung of 2.4 - 2.6 % | |
Elastizitätsmodul | 22.6 - 23.9 GPa Show Material materials with Elastizitätsmodul of 22.6 - 23.9 GPa | |
Zugfestigkeit | 450.0 - 490.0 MPa Show Material materials with Zugfestigkeit of 450.0 - 490.0 MPa | at 2.4-2.6% strain |
Thermisch
Property | Value |
---|---|
Koeffizient der thermischen Ausdehnung | 0.000013 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.000013 1/K |
Optisch
Property | Value |
---|---|
Transparenz | no |
Technological properties
Property | ||
---|---|---|
Application areas | Drones, bicycle seats, orthoses, back covers for electronics | |
Fillers | 45% Glass Fiber | |
Processing methods | Thermoforming, back injection molding |