Allgemein
Property | Value |
---|---|
Dichte | 0.88 - 1.24 g/cm³ Show Material materials with Dichte of 0.88 - 1.24 g/cm³ |
Mechanisch
Property | Value |
---|---|
Dehnung | 300.0 - 1800.0 % Show Material materials with Dehnung of 300.0 - 1800.0 % |
Zugfestigkeit | at 300-1800% strain |
Thermisch
Property | Value |
---|---|
Entflammbarkeit | UL 94 HB |
Optisch
Property | Value |
---|---|
Transparenz | yes |
Technological properties
Property | ||
---|---|---|
Application areas | Shoe solings, houseware grips, air bag covers, gaskets, pen grips | |
Other | You are viewing a generic polymer page, for more information please contact the suppliers or Matmatch, or use our Search under the following link to find more specific grades and formulations based on your application: Polymer Advanced Search | |
Processing methods | Injection molding, blow molding, extrusion, calandering, coating, compression molding |