Allgemein
Property | Value |
---|---|
Dichte | 1.03 - 1.05 g/cm³ Show Material materials with Dichte of 1.03 - 1.05 g/cm³ |
Mechanisch
Property | Value | Comment | |
---|---|---|---|
Elastizitätsmodul | 1.3 GPa Show Material materials with Elastizitätsmodul of 1.3 GPa | ||
Schlagfestigkeit, Charpy gekerbt | 12.0 - 24.0 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 12.0 - 24.0 kJ/m² | ||
Zugfestigkeit | 40 MPa Show Material materials with Zugfestigkeit of 40 MPa | at 5% strain | |
Schlagzähigkeit, Charpy ungekerbt | no break |
Thermisch
Property | Value |
---|---|
Schmelzpunkt | 190 °C Show Material materials with Schmelzpunkt of 190 °C |
Entflammbarkeit | UL 94 HB-V2 |
Optisch
Property | Value |
---|---|
Transparenz | yes |
Technological properties
Property | ||
---|---|---|
Application areas | Writing utensils, electronic components, winter sport equipment, mono- and multifilaments, textiles | |
Processing methods | Injection molding, extrusion, melt spin processes |