Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materialien
Categories
Sie sind nicht angemeldet
Categories
Metalllieferanten finden
List Your Company
Case Studies
Tools
Über uns
Poly-M-Xylylenadipamid (PAMXD6)
It is a crystalline polyamide produced by polycondensation of MXDA with adipic acid. Different from Nylon 6 and Nylon 66, Nylon-MXD6 is an aliphatic polyamide containing an aromatic ring in its main chain. Compared with Nylon 6 and Nylon 66, Nylon-MXD6 has the following favorable characteristics:
Diese Materialdaten wurden von M-Base zur Verfügung gestellt
See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
All categories
Let us help you find the best supplier!
Blow Moulding: History, Process, and Types
Difference between Biodegradable, Compostable, and Degradable
Fluoropolymers - The non-stick coating discovered by accident
LDPE vs HDPE: Properties, Production and Applications
Nylon Manufacturers and Suppliers
PETG vs PLA
Polyamide Nylon: Properties, Production and Applications
Polycarbonate (PC)
Polyether Ether Ketone (PEEK): Properties, Production, and Applications
Polyethylene (PE)
Polyimide: Properties, Processing, and Applications
Polypropylene: Properties, Processing, and Applications
Polytetrafluoroethylene (PTFE): Properties, Processing, and Applications
Polyvinyl Chloride (PVC): Properties, Processing, and Applications
Polyvinylidene Fluoride (PVDF): Properties, Production, & Applications
Styrene: Properties, Processing, and Applications
Thermoplastics vs. Thermosetting Polymers: Properties, Processing and Applications
What is Hostaform® M90XAP® POM?
What is Nylatron® GS?
What is Radel® R-5100?
What is Rilsan and what is it used for?
List your company on Matmatch now and reach engineers around the world looking for such materials.
Request more informationAllgemein
Property | Value |
---|---|
Dichte | 1.220 g/cm³ Show Material materials with Dichte of 1.220 g/cm³ |
Mechanisch
Property | Value |
---|---|
Elastizitätsmodul | 4.7 GPa Show Material materials with Elastizitätsmodul of 4.7 GPa |
Thermisch
Property | Value |
---|---|
Koeffizient der thermischen Ausdehnung | 0.000050 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 0.000050 1/K |
Schmelzpunkt | 235.0 - 240.0 °C Show Material materials with Schmelzpunkt of 235.0 - 240.0 °C |
Optisch
Property | Value |
---|---|
Transparenz | yes |
Technological properties
Property | ||
---|---|---|
Application areas | Monofilaments, food packaging, bottles, trays, cups | |
Processing methods | Injection molding, extrusion, blow molding |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
UNTERNEHMEN
KONTAKTIEREN SIE UNS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.