Vinyl ester (VE)

Alternative und Handelsbezeichungen
Atlac®, Epovia®
.XLSX
.PDF
Speichern

Beschreibung

It is a vinyl ester resin (Bisphenol-A epoxy based/Styrene-free/Brominated/Urethane modified) with excellent resistance against many chemicals at elevated temperatures. It brings great strength & toughness. It can be used in combination with a broad variety of fibers, including glass and carbon fibers

Eigenschaften

Allgemein

Density ρ

1.11 - 1.15 g/cm³ at 20 °C

Mechanisch

Elastic modulus E

3 - 4 GPa at 20 °C

Elongation A

2 - 7 % at 20 °C

Impact strength, Charpy unnotched Iunnot

15 - 30 kJ/m² at 20 °C

Max allowed stress σmax

60 - 95 MPa at 20 °C

at 2-7% strain

Thermisch

Max service temperature, long Tmaxlong

100 - 150 °C

Optisch

Transparency

no

Technische Eigenschaften

Application areas

Corrosion resistance parts, tanks relining, marine and swimming pool applications

Processing methods

Compression molding

Diese Materialdaten wurden von M-Base zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.