Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 3.51 g/cm³ Show Supplier Material materials with Dichte of 3.51 g/cm³ | |
Partikelgrößenbereich | 60 µm Show Supplier Material materials with Partikelgrößenbereich of 60 µm | Please refer to the technological properties section below for more detailed (narrow) particle size ranges available. |
Mechanisch
Property | Value |
---|---|
Härte, Mohs | 10 [-] Show Supplier Material materials with Härte, Mohs of 10 [-] |
Thermisch
Property | Value |
---|---|
Koeffizient der thermischen Ausdehnung | 1.1e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.1e-06 1/K |
Wärmeleitfähigkeit | 600 - 4000 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 600 - 4000 W/(m·K) |
Elektrisch
Property | Value |
---|---|
Bandabstand | 6 eV Show Supplier Material materials with Bandabstand of 6 eV |
spezifischer Widerstand | 1e+12 - 1e+19 Ω·m Show Supplier Material materials with spezifischer Widerstand of 1e+12 - 1e+19 Ω·m |
Optisch
Property | Value |
---|---|
Brechungsindex | 2 [-] Show Supplier Material materials with Brechungsindex of 2 [-] |
Chemical properties
Property | Value | Comment |
---|---|---|
Kohlenstoff | 99 % Show Supplier Material materials with Kohlenstoff of 99 % | min. purity |
Technological properties
Property | |||||||||||||||||||||||||||||||||||||||||||||||||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Application areas | MONO-ECO diamond is typically used for lapping of ceramics, metals and diamond wire dies. Examples of bonded applications include the use of MONO-ECO for wear-resistant surface coatings, for thermal conduction and for grinding tools. | ||||||||||||||||||||||||||||||||||||||||||||||||||||
Color | Yellowish Gray | ||||||||||||||||||||||||||||||||||||||||||||||||||||
Crystal structure | Monocrystalline | ||||||||||||||||||||||||||||||||||||||||||||||||||||
Gradings | Standard size range: The standard size range makes this product suitable for applications that focus primarily on cost. The controlled upper size limit ensures a uniform surface quality. | ||||||||||||||||||||||||||||||||||||||||||||||||||||
Particle size range table |
| ||||||||||||||||||||||||||||||||||||||||||||||||||||
Synthesis | MONO-ECO diamond is a monocrystalline metal-bond diamond produced by HPHT (high-pressure, high temperature) synthesis. The diamond particles feature an oriented crystal structure with parallel-running cleavage planes, similar to natural diamond. Depending on diamond size, MONO-ECO diamond varies in appearance from light gray to pale yellow. |