Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.3 g/cm³ Show Material materials with Dichte of 8.3 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 33.5 % Show Material materials with Dehnung of 33.5 % |
Flächenreduzierung | 20.0 °C | 36 % Show Material materials with Flächenreduzierung of 36 % |
760.0 °C | 14 % Show Material materials with Flächenreduzierung of 14 % | |
Streckgrenze | 20.0 °C | 660 MPa Show Material materials with Streckgrenze of 660 MPa |
650.0 °C | 590 MPa Show Material materials with Streckgrenze of 590 MPa | |
760.0 °C | 460 MPa Show Material materials with Streckgrenze of 460 MPa | |
Zugfestigkeit | 20.0 °C | 1030 MPa Show Material materials with Zugfestigkeit of 1030 MPa |
650.0 °C | 800 MPa Show Material materials with Zugfestigkeit of 800 MPa | |
760.0 °C | 460 MPa Show Material materials with Zugfestigkeit of 460 MPa | |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 760.0 °C | 1.49E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.49E-5 1/K | The mentioned value is between 20°C and the mentioned temperature |
Chemical properties
Property | Value |
---|---|
Chrom | 16 % Show Material materials with Chrom of 16 % |
Eisen | 77.98 - 100 % Show Material materials with Eisen of 77.98 - 100 % |
Kobalt | 0.5 % Show Material materials with Kobalt of 0.5 % |
Kohlenstoff | 0.04 % Show Material materials with Kohlenstoff of 0.04 % |
Kupfer | 0.1 % Show Material materials with Kupfer of 0.1 % |
Mangan | 2.25 % Show Material materials with Mangan of 2.25 % |
Silizium | 0.08 % Show Material materials with Silizium of 0.08 % |