Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8 - 8.3 g/cm³ Show Material materials with Dichte of 8 - 8.3 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A5 | 20.0 °C | 12 - 33 % Show Material materials with Dehnung A5 of 12 - 33 % |
Elastizitätsmodul | 20.0 °C | 215 GPa Show Material materials with Elastizitätsmodul of 215 GPa |
Flächenreduzierung | 20.0 °C | 20 - 32 % Show Material materials with Flächenreduzierung of 20 - 32 % |
Härte, Rockwell C | 20.0 °C | 32 - 40 [-] Show Material materials with Härte, Rockwell C of 32 - 40 [-] |
Streckgrenze | 20.0 °C | 630 - 850 MPa Show Material materials with Streckgrenze of 630 - 850 MPa |
Zugfestigkeit | 20.0 °C | 1100 - 1300 MPa Show Material materials with Zugfestigkeit of 1100 - 1300 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 1.3E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.3E-5 1/K | The mentioned values are between 20°C and the mentioned temperature |
200.0 °C | 1.3E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.3E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
300.0 °C | 1.4E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.4E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
500.0 °C | 1.45E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.45E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
600.0 °C | 1.4E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.4E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
700.0 °C | 1.55E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.55E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
1000.0 °C | 1.49E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.49E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
Spezifische Wärmekapazität | 20.0 °C | 460 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 J/(kg·K) | |
Wärmeleitfähigkeit | 20.0 °C | 13 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 13 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Aluminium | 1.1 - 1.35 % Show Material materials with Aluminium of 1.1 - 1.35 % |
Bor | 1.5E-3 - 9E-3 % Show Material materials with Bor of 1.5E-3 - 9E-3 % |
Chrom | 14 - 17 % Show Material materials with Chrom of 14 - 17 % |
Eisen | 5 - 9 % Show Material materials with Eisen of 5 - 9 % |
Kobalt | 1 % Show Material materials with Kobalt of 1 % |
Kohlenstoff | 0.03 - 0.1 % Show Material materials with Kohlenstoff of 0.03 - 0.1 % |
Mangan | 0.5 % Show Material materials with Mangan of 0.5 % |
Molybdän | 0.5 % Show Material materials with Molybdän of 0.5 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % |
Titan | 2 - 2.6 % Show Material materials with Titan of 2 - 2.6 % |