Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8 - 8.3 g/cm³ Show Material materials with Dichte of 8 - 8.3 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A5 | 20.0 °C | 15 - 40 % Show Material materials with Dehnung A5 of 15 - 40 % |
Elastizitätsmodul | 20.0 °C | 208 - 215 GPa Show Material materials with Elastizitätsmodul of 208 - 215 GPa |
Flächenreduzierung | 20.0 °C | 20 - 38 % Show Material materials with Flächenreduzierung of 20 - 38 % |
Härte, Rockwell C | 20.0 °C | 32 - 38 [-] Show Material materials with Härte, Rockwell C of 32 - 38 [-] |
Streckgrenze | 20.0 °C | 620 - 969 MPa Show Material materials with Streckgrenze of 620 - 969 MPa |
Zugfestigkeit | 20.0 °C | 1050 - 1400 MPa Show Material materials with Zugfestigkeit of 1050 - 1400 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 1.19E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.19E-5 1/K | The mentioned values are between 20°C and the mentioned temperature |
200.0 °C | 1.26E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.26E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
300.0 °C | 1.31E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.31E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
500.0 °C | 1.37E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.37E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
600.0 °C | 1.33E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.33E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
700.0 °C | 1.45E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.45E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
1000.0 °C | 1.39E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.39E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
Spezifische Wärmekapazität | 20.0 °C | 460 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 J/(kg·K) | |
Wärmeleitfähigkeit | 20.0 °C | 13 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 13 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Aluminium | 1 - 1.8 % Show Material materials with Aluminium of 1 - 1.8 % |
Bor | 8E-3 % Show Material materials with Bor of 8E-3 % |
Chrom | 18 - 21 % Show Material materials with Chrom of 18 - 21 % |
Eisen | 3 % Show Material materials with Eisen of 3 % |
Kohlenstoff | 0.04 - 0.1 % Show Material materials with Kohlenstoff of 0.04 - 0.1 % |
Kupfer | 0.2 % Show Material materials with Kupfer of 0.2 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |
Titan | 1.8 - 2.7 % Show Material materials with Titan of 1.8 - 2.7 % |