Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 22 - 26 % Show Material materials with Chrom of 22 - 26 % | |
Eisen | 56.25 - 100 % Show Material materials with Eisen of 56.25 - 100 % | Balance |
Kohlenstoff | 2 - 2.5 % Show Material materials with Kohlenstoff of 2 - 2.5 % | |
Molybdän | 5 - 6 % Show Material materials with Molybdän of 5 - 6 % | |
Nickel | 10 - 12 % Show Material materials with Nickel of 10 - 12 % | |
Silizium | 0.8 - 1.3 % Show Material materials with Silizium of 0.8 - 1.3 % |