Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 9 g/cm³ Show Material materials with Dichte of 9 g/cm³ | Typical for Cobalt Superalloy |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 6E-7 - 8.7E-6 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 6E-7 - 8.7E-6 1/K | Typical for Cobalt Superalloy |
Chemical properties
Property | Value |
---|---|
Chrom | 26 - 33 % Show Material materials with Chrom of 26 - 33 % |
Eisen | 3 % Show Material materials with Eisen of 3 % |
Kohlenstoff | 1.1 - 1.7 % Show Material materials with Kohlenstoff of 1.1 - 1.7 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Molybdän | 1 % Show Material materials with Molybdän of 1 % |
Nickel | 3 % Show Material materials with Nickel of 3 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 0.4 - 2 % Show Material materials with Silizium of 0.4 - 2 % |
Wolfram | 7 - 9.5 % Show Material materials with Wolfram of 7 - 9.5 % |