Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 8.3 g/cm³ Show Material materials with Dichte of 8.3 g/cm³ | Typical for Cobalt Chromium Molybdenum |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1E-5 - 1.5E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1E-5 - 1.5E-5 1/K | Typical for Cobalt Chromium Molybdenum |
Chemical properties
Property | Value |
---|---|
Chrom | 7.5 - 10 % Show Material materials with Chrom of 7.5 - 10 % |
Eisen | 3 % Show Material materials with Eisen of 3 % |
Kobalt | 61 - 63 % Show Material materials with Kobalt of 61 - 63 % |
Kohlenstoff | 0.08 % Show Material materials with Kohlenstoff of 0.08 % |
Molybdän | 26.5 - 30 % Show Material materials with Molybdän of 26.5 - 30 % |
Nickel | 3 % Show Material materials with Nickel of 3 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 2.2 - 3 % Show Material materials with Silizium of 2.2 - 3 % |