Mechanisch
Property | Temperature | Value |
---|---|---|
Flächenreduzierung | 23.0 °C | 15 % Show Material materials with Flächenreduzierung of 15 % |
Härte, Rockwell C | 23.0 °C | 32 - 45 [-] Show Material materials with Härte, Rockwell C of 32 - 45 [-] |
Streckgrenze | 23.0 °C | 1030 MPa Show Material materials with Streckgrenze of 1030 MPa |
Zugfestigkeit | 23.0 °C | 1280 MPa Show Material materials with Zugfestigkeit of 1280 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 1.2 - 1.6 % Show Material materials with Aluminium of 1.2 - 1.6 % |
Bor | 0.003 - 0.01 % Show Material materials with Bor of 0.003 - 0.01 % |
Chrom | 18 - 21 % Show Material materials with Chrom of 18 - 21 % |
Eisen | 2 % Show Material materials with Eisen of 2 % |
Kobalt | 12 - 15 % Show Material materials with Kobalt of 12 - 15 % |
Kohlenstoff | 0.03 - 0.1 % Show Material materials with Kohlenstoff of 0.03 - 0.1 % |
Kupfer | 0.5 % Show Material materials with Kupfer of 0.5 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Molybdän | 3.5 - 5 % Show Material materials with Molybdän of 3.5 - 5 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 0.75 % Show Material materials with Silizium of 0.75 % |
Titan | 2.75 - 3.5 % Show Material materials with Titan of 2.75 - 3.5 % |
Zirkonium | 0.02 - 0.12 % Show Material materials with Zirkonium of 0.02 - 0.12 % |