Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 18 % Show Material materials with Dehnung A50 of 18 % |
Härte, Brinell | 20.0 °C | 217 [-] Show Material materials with Härte, Brinell of 217 [-] |
Yield Strength Rp0.2, short transverse | 20.0 °C | 585 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 585 MPa |
Zugfestigkeit | 20.0 °C | 725 - 895 MPa Show Material materials with Zugfestigkeit of 725 - 895 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 1.5 - 2 % Show Material materials with Chrom of 1.5 - 2 % |
Kohlenstoff | 0.23 % Show Material materials with Kohlenstoff of 0.23 % |
Mangan | 0.2 - 0.4 % Show Material materials with Mangan of 0.2 - 0.4 % |
Molybdän | 0.4 - 0.6 % Show Material materials with Molybdän of 0.4 - 0.6 % |
Nickel | 2.8 - 3.9 % Show Material materials with Nickel of 2.8 - 3.9 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.01 % Show Material materials with Schwefel of 0.01 % |
Silizium | 0.3 % Show Material materials with Silizium of 0.3 % |
Vanadium | 0.08 % Show Material materials with Vanadium of 0.08 % |