Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 3.2 g/cm³ Show Material materials with Dichte of 3.2 g/cm³ | Typical for Ferrosilicon |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 1250 GPa Show Material materials with Elastizitätsmodul of 1250 GPa | Typical for Ferrosilicon |
Thermisch
Property | Value | Comment |
---|---|---|
Schmelzpunkt | 1200 °C Show Material materials with Schmelzpunkt of 1200 °C | Typical for Ferrosilicon |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.5 % Show Material materials with Aluminium of 0.5 % |
Kohlenstoff | 0.1 % Show Material materials with Kohlenstoff of 0.1 % |
Mangan | 0.4 % Show Material materials with Mangan of 0.4 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % |
Silizium | 74 - 79 % Show Material materials with Silizium of 74 - 79 % |