Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.9 g/cm³ Show Material materials with Dichte of 8.9 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 18 % Show Material materials with Dehnung of 18 % | |
Elastizitätsmodul | 20.0 °C | 123 GPa Show Material materials with Elastizitätsmodul of 123 GPa | |
Härte, Brinell | 20.0 °C | 100 [-] Show Material materials with Härte, Brinell of 100 [-] | |
Poissonzahl | 23.0 °C | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | Typical for Cast Copper Nickel Grade |
Streckgrenze Rp 0,2 | 20.0 °C | 150 MPa Show Material materials with Streckgrenze Rp 0,2 of 150 MPa | |
Zugfestigkeit | 20.0 °C | 310 MPa Show Material materials with Zugfestigkeit of 310 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 300.0 °C | 1.7E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.7E-5 1/K | |
Schmelzpunkt | 1100 - 1240 °C Show Material materials with Schmelzpunkt of 1100 - 1240 °C | Typical for Cast Copper Nickel Grade | |
Spezifische Wärmekapazität | 23.0 °C | 377 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 377 J/(kg·K) | Typical for Cast Copper Nickel Grade |
Wärmeleitfähigkeit | 20.0 °C | 59 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 59 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 5.50E+6 S/m Show Material materials with Elektrische Leitfähigkeit of 5.50E+6 S/m |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 % Show Material materials with Aluminium of 0.01 % |
Bismut | 0.01 % Show Material materials with Bismut of 0.01 % |
Blei | 0.01 % Show Material materials with Blei of 0.01 % |
Bor | 0.01 % Show Material materials with Bor of 0.01 % |
Cadmium | 0.02 % Show Material materials with Cadmium of 0.02 % |
Eisen | 1 - 1.8 % Show Material materials with Eisen of 1 - 1.8 % |
Kohlenstoff | 0.03 % Show Material materials with Kohlenstoff of 0.03 % |
Kupfer | 84.5 % Show Material materials with Kupfer of 84.5 % |
Magnesium | 0.01 % Show Material materials with Magnesium of 0.01 % |
Mangan | 1 - 1.5 % Show Material materials with Mangan of 1 - 1.5 % |
Nickel | 9 - 11 % Show Material materials with Nickel of 9 - 11 % |
Niobium | 0.15 - 0.35 % Show Material materials with Niobium of 0.15 - 0.35 % |
Phosphor | 0.01 % Show Material materials with Phosphor of 0.01 % |
Schwefel | 0.01 % Show Material materials with Schwefel of 0.01 % |
Selen | 0.01 % Show Material materials with Selen of 0.01 % |
Silizium | 0.15 - 0.25 % Show Material materials with Silizium of 0.15 - 0.25 % |
Tellur | 0.01 % Show Material materials with Tellur of 0.01 % |
Zink | 0.5 % Show Material materials with Zink of 0.5 % |
Technological properties
Property | ||
---|---|---|
Processing methods | sand casting, separately cast test sample |