Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 1.74 g/cm³ Show Material materials with Dichte of 1.74 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 20.0 °C | 45 GPa Show Material materials with Elastizitätsmodul of 45 GPa | |
Härte, Brinell | 20.0 °C | 38 [-] Show Material materials with Härte, Brinell of 38 [-] | |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Magnesium |
Schubmodule | 23.0 °C | 45 GPa Show Material materials with Schubmodule of 45 GPa | Typical for Magnesium |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.3E-5 - 2.6E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.3E-5 - 2.6E-5 1/K | Typical for Magnesium |
Schmelzpunkt | 650 °C Show Material materials with Schmelzpunkt of 650 °C | Typical for Magnesium | |
Spezifische Wärmekapazität | 23.0 °C | 1010 - 1060 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 1010 - 1060 J/(kg·K) | Typical for Magnesium |
Wärmeleitfähigkeit | 20.0 °C | 155 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 155 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 2.24E+7 S/m Show Material materials with Elektrische Leitfähigkeit of 2.24E+7 S/m |
Chemical properties
Property | Value |
---|---|
Eisen | 0.05 % Show Material materials with Eisen of 0.05 % |
Kupfer | 0.02 % Show Material materials with Kupfer of 0.02 % |
Magnesium | 99.8 % Show Material materials with Magnesium of 99.8 % |
Mangan | 0.1 % Show Material materials with Mangan of 0.1 % |
Nickel | 2E-3 % Show Material materials with Nickel of 2E-3 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |