Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 8.9 g/cm³ Show Material materials with Dichte of 8.9 g/cm³ | Typical for Pure/Low Nickel Alloy |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 40 % Show Material materials with Dehnung of 40 % | |
Elastizitätsmodul | 23.0 °C | 190 - 220 GPa Show Material materials with Elastizitätsmodul of 190 - 220 GPa | Typical for Pure/Low Nickel Alloy |
Elongation A100 | 20.0 °C | 20 - 30 % Show Material materials with Elongation A100 of 20 - 30 % | |
Zugfestigkeit | 20.0 °C | 340 - 400 MPa Show Material materials with Zugfestigkeit of 340 - 400 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 8.5E-6 - 1.4E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 8.5E-6 - 1.4E-5 1/K | Typical for Pure/Low Nickel Alloy |
Schmelzpunkt | 1400 - 1500 °C Show Material materials with Schmelzpunkt of 1400 - 1500 °C | Typical for Pure/Low Nickel Alloy | |
Spezifische Wärmekapazität | 23.0 °C | 430 - 532 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 430 - 532 J/(kg·K) | Typical for Pure/Low Nickel Alloy |
Wärmeleitfähigkeit | 23.0 °C | 18 - 86 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 18 - 86 W/(m·K) | Typical for Pure/Low Nickel Alloy |
Chemical properties
Property | Value |
---|---|
Eisen | 0.5 % Show Material materials with Eisen of 0.5 % |
Kobalt | 1 % Show Material materials with Kobalt of 1 % |
Kohlenstoff | 0.15 - 0.25 % Show Material materials with Kohlenstoff of 0.15 - 0.25 % |
Kupfer | 0.5 % Show Material materials with Kupfer of 0.5 % |
Magnesium | 0.15 % Show Material materials with Magnesium of 0.15 % |
Mangan | 0.7 - 1.3 % Show Material materials with Mangan of 0.7 - 1.3 % |
Nickel | 97 % Show Material materials with Nickel of 97 % |
Schwefel | 0.01 % Show Material materials with Schwefel of 0.01 % |
Silizium | 0.25 % Show Material materials with Silizium of 0.25 % |
Titan | 0.1 % Show Material materials with Titan of 0.1 % |