Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 30 - 40 % Show Material materials with Dehnung of 30 - 40 % |
Elongation A100 | 20.0 °C | 30 % Show Material materials with Elongation A100 of 30 % |
Streckgrenze Rp 0,2 | 20.0 °C | 140 MPa Show Material materials with Streckgrenze Rp 0,2 of 140 MPa |
Streckgrenze Rp 1,0 | 20.0 °C | 170 MPa Show Material materials with Streckgrenze Rp 1,0 of 170 MPa |
Zugfestigkeit | 20.0 °C | 400 - 420 MPa Show Material materials with Zugfestigkeit of 400 - 420 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 1.4 - 1.8 % Show Material materials with Chrom of 1.4 - 1.8 % |
Eisen | 0.3 % Show Material materials with Eisen of 0.3 % |
Kobalt | 1 % Show Material materials with Kobalt of 1 % |
Kohlenstoff | 0.05 % Show Material materials with Kohlenstoff of 0.05 % |
Kupfer | 0.15 % Show Material materials with Kupfer of 0.15 % |
Mangan | 1.3 - 1.8 % Show Material materials with Mangan of 1.3 - 1.8 % |
Nickel | 94.5 % Show Material materials with Nickel of 94.5 % |
Schwefel | 5E-3 % Show Material materials with Schwefel of 5E-3 % |
Silizium | 0.4 - 0.65 % Show Material materials with Silizium of 0.4 - 0.65 % |
Titan | 0.1 % Show Material materials with Titan of 0.1 % |