Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.18 g/cm³ Show Material materials with Dichte of 7.18 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 105 GPa Show Material materials with Elastizitätsmodul of 105 GPa | Typical for Zinc |
Elongation A10 | 20.0 °C | 20 % Show Material materials with Elongation A10 of 20 % | |
Härte, Brinell | 20.0 °C | 40 [-] Show Material materials with Härte, Brinell of 40 [-] | |
Poissonzahl | 23.0 °C | 0.25 [-] Show Material materials with Poissonzahl of 0.25 [-] | Typical for Zinc |
Schubmodule | 23.0 °C | 42 GPa Show Material materials with Schubmodule of 42 GPa | Typical for Zinc |
Zugfestigkeit | 20.0 °C | 180 MPa Show Material materials with Zugfestigkeit of 180 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.2E-5 - 2.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.2E-5 - 2.8E-5 1/K | Typical for Zinc |
Schmelzpunkt | 380 - 420 °C Show Material materials with Schmelzpunkt of 380 - 420 °C | Typical for Zinc | |
Spezifische Wärmekapazität | 23.0 °C | 272 - 525 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 272 - 525 J/(kg·K) | Typical for Zinc |
Wärmeleitfähigkeit | 23.0 °C | 105 - 125 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 105 - 125 W/(m·K) | Typical for Zinc |