Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.14 g/cm³ Show Material materials with Dichte of 7.14 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 105 GPa Show Material materials with Elastizitätsmodul of 105 GPa | Typical for Zinc |
Elongation A10 | 20.0 °C | 50 % Show Material materials with Elongation A10 of 50 % | |
Härte, Brinell | 20.0 °C | 30 [-] Show Material materials with Härte, Brinell of 30 [-] | |
Poissonzahl | 23.0 °C | 0.25 [-] Show Material materials with Poissonzahl of 0.25 [-] | Typical for Zinc |
Schubmodule | 23.0 °C | 42 GPa Show Material materials with Schubmodule of 42 GPa | Typical for Zinc |
Zugfestigkeit | 20.0 °C | 120 MPa Show Material materials with Zugfestigkeit of 120 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.2E-5 - 2.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.2E-5 - 2.8E-5 1/K | Typical for Zinc |
Schmelzpunkt | 380 - 420 °C Show Material materials with Schmelzpunkt of 380 - 420 °C | Typical for Zinc | |
Spezifische Wärmekapazität | 20.0 °C | 380 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 380 J/(kg·K) | |
Wärmeleitfähigkeit | 20.0 °C | 113 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 113 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Blei | 3E-3 % Show Material materials with Blei of 3E-3 % |
Cadmium | 3E-3 % Show Material materials with Cadmium of 3E-3 % |
Eisen | 2E-3 % Show Material materials with Eisen of 2E-3 % |
Kupfer | 1E-3 % Show Material materials with Kupfer of 1E-3 % |
Zink | 100 % Show Material materials with Zink of 100 % |
Zinn | 1E-3 % Show Material materials with Zinn of 1E-3 % |