Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 2.75 g/cm³ Show Material materials with Dichte of 2.75 g/cm³ | Typical for Cast 1xx.x Series Aluminium |
Mechanisch
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.8e-05 - 2.4e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.8e-05 - 2.4e-05 1/K | Typical for Cast 1xx.x Series Aluminium |
Schmelzpunkt | 643.0 - 657.0 °C Show Material materials with Schmelzpunkt of 643.0 - 657.0 °C | Typical for Cast 1xx.x Series Aluminium |
Wärmeleitfähigkeit | 209.0 - 222.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 209.0 - 222.0 W/(m·K) | Typical for Cast 1xx.x Series Aluminium |
Chemical properties
Property | Value | Related Standards |
---|---|---|
Aluminium | 99.99 % Show Material materials with Aluminium of 99.99 % | EN 576 |
Eisen | 0.005 % Show Material materials with Eisen of 0.005 % | DIN 1712-1, EN 576 |
0.005 % Show Material materials with Eisen of 0.005 % | EN 576 | |
Kupfer | 0.003 % Show Material materials with Kupfer of 0.003 % | DIN 1712-1, EN 576 |
Silizium | 0.006 % Show Material materials with Silizium of 0.006 % | DIN 1712-1, EN 576 |
0.01 % Show Material materials with Silizium of 0.01 % | EN 576 | |
Titan | 0.002 % Show Material materials with Titan of 0.002 % | DIN 1712-1, EN 576 |
Zink | 0.005 % Show Material materials with Zink of 0.005 % | DIN 1712-1, EN 576 |