Allgemein
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Dehnung | 20.0 °C | 22.0 % Show Material materials with Dehnung of 22.0 % | F | DIN 1712-3, EN 573-3, EN 573-4 | Profile, Rod, Tube | A10 |
20.0 °C | 25.0 % Show Material materials with Dehnung of 25.0 % | F | DIN 1712-3, EN 573-3, EN 573-4 | Profile, Rod, Tube | ||
Elastizitätsmodul | 70.0 GPa Show Material materials with Elastizitätsmodul of 70.0 GPa | F | EN 573-3, EN 1715-3, EN 1715-4, EN 485, EN 570 | |||
20.0 °C | 60.0 - 70.0 GPa Show Material materials with Elastizitätsmodul of 60.0 - 70.0 GPa | F | DIN 1712-3, EN 573-3, EN 573-4 | Profile, Rod, Tube | ||
Härte, Brinell | 18.0 [-] Show Material materials with Härte, Brinell of 18.0 [-] | F | EN 573-3, EN 485 | |||
19.0 [-] Show Material materials with Härte, Brinell of 19.0 [-] | F | EN 573-3, EN 570 | ||||
20.0 °C | 18.0 [-] Show Material materials with Härte, Brinell of 18.0 [-] | F | DIN 1712-3, EN 573-3, EN 573-4 | Profile, Rod, Tube | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 1000 Series Aluminium | ||||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 1000 Series Aluminium | ||||
Schubmodule | 20.0 °C | 25.0 GPa Show Material materials with Schubmodule of 25.0 GPa | F | DIN 1712-3, EN 573-3, EN 573-4 | Profile, Rod, Tube | |
Zugfestigkeit | 60.0 MPa Show Material materials with Zugfestigkeit of 60.0 MPa | F | EN 573-3, EN 485 | |||
80.0 - 110.0 MPa Show Material materials with Zugfestigkeit of 80.0 - 110.0 MPa | F | EN 573-3, EN 1715-3, EN 1715-4 | ||||
20.0 °C | 55.0 MPa Show Material materials with Zugfestigkeit of 55.0 MPa | F | DIN 1712-3, EN 573-3, EN 573-4 | Profile | ||
20.0 °C | 60.0 MPa Show Material materials with Zugfestigkeit of 60.0 MPa | F | DIN 1712-3, EN 573-3, EN 573-4 | Rod, Tube |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20 °C | 2.35e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.35e-05 1/K | F | EN 573-3, EN 1715-3, EN 1715-4, EN 485, EN 570 | |
100 °C | 2.35e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.35e-05 1/K | F | EN 573-3, EN 1715-3, EN 1715-4, EN 485, EN 570 | ||
Schmelzpunkt | 659.0 °C Show Material materials with Schmelzpunkt of 659.0 °C | F | EN 573-3, EN 1715-3, EN 1715-4, EN 485, EN 570 | ||
Spezifische Wärmekapazität | 20.0 °C | 921.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 921.0 J/(kg·K) | F | DIN 1712-3, EN 573-3, EN 573-4 | Profile, Rod, Tube |
Wärmeleitfähigkeit | 225 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 225 W/(m·K) | F | EN 573-3, EN 1715-3, EN 1715-4, EN 485, EN 570 | ||
20.0 °C | 215.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 215.0 W/(m·K) | F | DIN 1712-3, EN 573-3, EN 573-4 | Profile, Rod, Tube |
Elektrisch
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Elektrische Leitfähigkeit | 34500000.0 - 35000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 34500000.0 - 35000000.0 S/m | F | EN 573-3, EN 1715-3, EN 1715-4, EN 485, EN 570 | ||
20.0 °C | 36400000.0 - 37000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 36400000.0 - 37000000.0 S/m | F | DIN 1712-3, EN 573-3, EN 573-4 | Profile, Rod, Tube | |
spezifischer Widerstand | 2.86e-08 - 2.9e-08 Ω·m Show Material materials with spezifischer Widerstand of 2.86e-08 - 2.9e-08 Ω·m | F | EN 573-3, EN 1715-3, EN 1715-4, EN 485, EN 570 |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminium | 99.8 % Show Material materials with Aluminium of 99.8 % | F | EN 573-3, EN 1715-3, EN 1715-4, EN 485, EN 570 | |
Eisen | 0.15 % Show Material materials with Eisen of 0.15 % | F | DIN 1712-3, EN 573-3, EN 573-4 | Profile, Rod, Tube |
0.15 % Show Material materials with Eisen of 0.15 % | F | EN 573-3, EN 1715-3, EN 1715-4, EN 485, EN 570 | ||
Gallium | 0.03 % Show Material materials with Gallium of 0.03 % | F | DIN 1712-3, EN 573-3, EN 573-4, EN 1715-3, EN 1715-4, EN 485, EN 570 | Profile, Rod, Tube |
Kupfer | 0.03 % Show Material materials with Kupfer of 0.03 % | F | DIN 1712-3, EN 573-3, EN 573-4, EN 1715-3, EN 1715-4, EN 485, EN 570 | Profile, Rod, Tube |
Magnesium | 0.02 % Show Material materials with Magnesium of 0.02 % | F | DIN 1712-3, EN 573-3, EN 573-4, EN 1715-3, EN 1715-4, EN 485, EN 570 | Profile, Rod, Tube |
Mangan | 0.02 % Show Material materials with Mangan of 0.02 % | F | DIN 1712-3, EN 573-3, EN 573-4, EN 1715-3, EN 1715-4, EN 485, EN 570 | Profile, Rod, Tube |
Silizium | 0.15 % Show Material materials with Silizium of 0.15 % | F | DIN 1712-3, EN 573-3, EN 573-4, EN 1715-3, EN 1715-4, EN 485, EN 570 | Profile, Rod, Tube |
Titan | 0.02 % Show Material materials with Titan of 0.02 % | F | DIN 1712-3, EN 573-3, EN 573-4, EN 1715-3, EN 1715-4, EN 485, EN 570 | Profile, Rod, Tube |
Zink | 0.06 % Show Material materials with Zink of 0.06 % | F | DIN 1712-3, EN 573-3, EN 573-4, EN 1715-3, EN 1715-4, EN 485, EN 570 | Profile, Rod, Tube |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: very good, Protective: very good | |
Brazing | hard brazing (with flux/ without flux): very good / very good, friction soldering: very good, soft brazing with flux: very good | |
Workability | Bending / Spinning (cold): very good / very good, Impact extrusion (cold): very good, Deep drawing / upsetting (Condition) very good (H14) / very good (H12) |