DIN 1725-1 Grade 3.3210 T8

View suppliers (1)
Want to keep this datasheet? Save it now in your required format

Description

This cold and hot hardenable material reaches mechanical properties from 200 to 250 MPa with A5-elongations at break of approx. 10 %. In warm and cold-hardened condition is this alloy only limited ductile, in the soft material condition however well. The Weldability, the corrosion resistance and the ability for anodising are good. However this alloy is used more for rivet or bolt joints, because of the destabilization arising within the welding seam range. Heat treatment for hardening: solution annealing: 525 to 540 °C, quenching on air or in water cold ageing: 5 to 8 d at ambient temperature hot ageing: 4 to 16 h at 155 to 190 °C Application: In the construction of vehicles for vehicle floors, bordwaende, stands, commercial motor vehicle superstructures of all kinds, trim. In the building industry for window, doors, window walls, shower cubicles, fences. In the building of rail-mounted vehicles for car boxes. In shipbuilding for sail masts, sail trees. In mechanical engineering (including building of forms) and for metal goods (e.g. building fittings, table-ware, flow pressed parts, reflectors).

Related Standards

Equivalent Materials

Diese Materialdaten wurden von WIAM zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Eigenschaften

Allgemein

PropertyTemperatureValueConditionRelated StandardsShape

Dichte

20.0 °C

2.7 g/cm³

Show Material materials with Dichte of 2.7 g/cm³

T8

DIN 1725-1, EN 573-3, EN 573-4

Profile, Tube

Mechanisch

PropertyTemperatureValueConditionRelated StandardsShapeComment

Dehnung

20.0 °C

6.0 %

Show Material materials with Dehnung of 6.0 %

T8

DIN 1725-1, EN 573-3, EN 573-4

Profile, Tube

A10

20.0 °C

8.0 %

Show Material materials with Dehnung of 8.0 %

T8

DIN 1725-1, EN 573-3, EN 573-4

Profile, Tube

Elastizitätsmodul

20.0 °C

73.0

Show Material materials with Elastizitätsmodul of 73.0

T8

DIN 1725-1, EN 573-3, EN 573-4

Profile, Tube

Härte, Brinell

20.0 °C

85.0 [-]

Show Material materials with Härte, Brinell of 85.0 [-]

T8

DIN 1725-1, EN 573-3, EN 573-4

Profile, Tube

20.0 °C

90.0 [-]

Show Material materials with Härte, Brinell of 90.0 [-]

T8

DIN 1725-1, EN 573-3, EN 573-4

Profile

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 6000 Series Aluminium

Poissonzahl

0.33 [-]

Show Material materials with Poissonzahl of 0.33 [-]

Typical for Wrought 6000 Series Aluminium

Schubmodule

20.0 °C

27.0

Show Material materials with Schubmodule of 27.0

T8

DIN 1725-1, EN 573-3, EN 573-4

Profile, Tube

Zugfestigkeit

20.0 °C

260.0 MPa

Show Material materials with Zugfestigkeit of 260.0 MPa

T8

DIN 1725-1, EN 573-3, EN 573-4

Profile, Tube

20.0 °C

270.0 MPa

Show Material materials with Zugfestigkeit of 270.0 MPa

T8

DIN 1725-1, EN 573-3, EN 573-4

Profile

Thermisch

PropertyTemperatureValueConditionRelated StandardsShapeComment

Koeffizient der thermischen Ausdehnung

1.6e-05 - 2.4e-05 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6e-05 - 2.4e-05 1/K

Typical for Wrought 6000 Series Aluminium

Schmelzpunkt

555.0 - 655.0 °C

Show Material materials with Schmelzpunkt of 555.0 - 655.0 °C

Typical for Wrought 6000 Series Aluminium

Spezifische Wärmekapazität

887.0 - 963.0 J/(kg·K)

Show Material materials with Spezifische Wärmekapazität of 887.0 - 963.0 J/(kg·K)

Typical for Wrought 6000 Series Aluminium

Wärmeleitfähigkeit

20.0 °C

170.0 - 220.0 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 170.0 - 220.0 W/(m·K)

T8

DIN 1725-1, EN 573-3, EN 573-4

Profile, Tube

Elektrisch

PropertyTemperatureValueConditionRelated StandardsShapeComment

Elektrische Leitfähigkeit

20.0 °C

24000000.0 - 32000000.0 S/m

Show Material materials with Elektrische Leitfähigkeit of 24000000.0 - 32000000.0 S/m

T8

DIN 1725-1, EN 573-3, EN 573-4

Profile, Tube

spezifischer Widerstand

2.9e-08 - 5e-08 Ω·m

Show Material materials with spezifischer Widerstand of 2.9e-08 - 5e-08 Ω·m

Typical for Wrought 6000 Series Aluminium

Chemical properties

PropertyValueConditionRelated StandardsShape

Chrom

0.3

Show Material materials with Chrom of 0.3

T8

DIN 1725-1, EN 573-3, EN 573-4

Profile, Tube

Eisen

0.35

Show Material materials with Eisen of 0.35

T8

DIN 1725-1, EN 573-3, EN 573-4

Profile, Tube

Kupfer

0.3

Show Material materials with Kupfer of 0.3

T8

DIN 1725-1, EN 573-3, EN 573-4

Profile, Tube

Magnesium

0.4 - 0.7 %

Show Material materials with Magnesium of 0.4 - 0.7 %

T8

DIN 1725-1, EN 573-3, EN 573-4

Profile, Tube

Mangan

0.5

Show Material materials with Mangan of 0.5

T8

DIN 1725-1, EN 573-3, EN 573-4

Profile, Tube

Silizium

0.5 - 0.9 %

Show Material materials with Silizium of 0.5 - 0.9 %

T8

DIN 1725-1, EN 573-3, EN 573-4

Profile, Tube

Titan

0.1

Show Material materials with Titan of 0.1

T8

DIN 1725-1, EN 573-3, EN 573-4

Profile, Tube

Zink

0.2

Show Material materials with Zink of 0.2

T8

DIN 1725-1, EN 573-3, EN 573-4

Profile, Tube

Technological properties

Property
Workability

Excellent workability.