Allgemein
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Dichte | 20.0 °C | 2.75 g/cm³ Show Material materials with Dichte of 2.75 g/cm³ | T3 | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Tube |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Dehnung | 20.0 °C | 8.0 % Show Material materials with Dehnung of 8.0 % | T3 | DIN 1725-1, EN 573-3, EN 573-4 | Rod | A10 |
20.0 °C | 10.0 % Show Material materials with Dehnung of 10.0 % | T3 | DIN 1725-1, EN 573-3, EN 573-4 | Tube | A10 | |
20.0 °C | 10.0 % Show Material materials with Dehnung of 10.0 % | T3 | DIN 1725-1, EN 573-3, EN 573-4 | Rod | ||
20.0 °C | 12.0 % Show Material materials with Dehnung of 12.0 % | T3 | DIN 1725-1, EN 573-3, EN 573-4 | Tube | ||
Elastizitätsmodul | 70.0 GPa Show Material materials with Elastizitätsmodul of 70.0 GPa | Typical for Wrought 6000 Series Aluminium | ||||
Härte, Brinell | 20.0 °C | 60.0 [-] Show Material materials with Härte, Brinell of 60.0 [-] | T3 | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Tube | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 6000 Series Aluminium | ||||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 6000 Series Aluminium | ||||
Schubmodule | 26.0 - 26.5 GPa Show Material materials with Schubmodule of 26.0 - 26.5 GPa | Typical for Wrought 6000 Series Aluminium | ||||
Zugfestigkeit | 20.0 °C | 200.0 MPa Show Material materials with Zugfestigkeit of 200.0 MPa | T3 | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Tube |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 2.3e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3e-05 1/K | T3 | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Tube | |
Schmelzpunkt | 555.0 - 655.0 °C Show Material materials with Schmelzpunkt of 555.0 - 655.0 °C | Typical for Wrought 6000 Series Aluminium | ||||
Spezifische Wärmekapazität | 887.0 - 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 887.0 - 963.0 J/(kg·K) | Typical for Wrought 6000 Series Aluminium | ||||
Wärmeleitfähigkeit | 20.0 °C | 163.0 - 186.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 163.0 - 186.0 W/(m·K) | T3 | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Tube |
Elektrisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 24000000.0 - 28000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 24000000.0 - 28000000.0 S/m | T3 | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Tube | |
spezifischer Widerstand | 2.9e-08 - 5e-08 Ω·m Show Material materials with spezifischer Widerstand of 2.9e-08 - 5e-08 Ω·m | Typical for Wrought 6000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Bismut | 0.7 Show Material materials with Bismut of 0.7 | T3 | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Tube |
Blei | 0.4 - 2.0 % Show Material materials with Blei of 0.4 - 2.0 % | T3 | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Tube |
Chrom | 0.3 Show Material materials with Chrom of 0.3 | T3 | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Tube |
Eisen | 0.5 Show Material materials with Eisen of 0.5 | T3 | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Tube |
Kupfer | 0.1 Show Material materials with Kupfer of 0.1 | T3 | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Tube |
Magnesium | 0.6 - 1.2 % Show Material materials with Magnesium of 0.6 - 1.2 % | T3 | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Tube |
Mangan | 0.4 - 1.0 % Show Material materials with Mangan of 0.4 - 1.0 % | T3 | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Tube |
Silizium | 0.6 - 1.4 % Show Material materials with Silizium of 0.6 - 1.4 % | T3 | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Tube |
Titan | 0.2 Show Material materials with Titan of 0.2 | T3 | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Tube |
Zink | 0.3 Show Material materials with Zink of 0.3 | T3 | DIN 1725-1, EN 573-3, EN 573-4 | Rod, Tube |
Technological properties
Property | ||
---|---|---|
Workability | Excellent workability. |