Chemical properties
Property | Value | Related Standards |
---|---|---|
Blei | 0.02 % Show Material materials with Blei of 0.02 % | EN 575, DIN 1725-3 |
Bor | 0.01 % Show Material materials with Bor of 0.01 % | EN 575, DIN 1725-3 |
Eisen | 0.5 % Show Material materials with Eisen of 0.5 % | EN 575, DIN 1725-3 |
0.50 % Show Material materials with Eisen of 0.50 % | EN 575 | |
Kalzium | 0.15 % Show Material materials with Kalzium of 0.15 % | EN 575, DIN 1725-3 |
Silizium | 47.0 - 53.0 % Show Material materials with Silizium of 47.0 - 53.0 % | EN 575, DIN 1725-3 |
Zink | 0.04 % Show Material materials with Zink of 0.04 % | EN 575, DIN 1725-3 |
Zinn | 0.02 % Show Material materials with Zinn of 0.02 % | EN 575, DIN 1725-3 |