Chemical properties
Property | Value | Related Standards |
---|---|---|
Chrom | 0.1 % Show Material materials with Chrom of 0.1 % | EN 575, DIN 1725-3 |
Eisen | 0.7 % Show Material materials with Eisen of 0.7 % | EN 575, DIN 1725-3 |
0.70 % Show Material materials with Eisen of 0.70 % | EN 575 | |
Kupfer | 0.2 % Show Material materials with Kupfer of 0.2 % | EN 575, DIN 1725-3 |
Magnesium | 0.5 % Show Material materials with Magnesium of 0.5 % | EN 575, DIN 1725-3 |
Mangan | 0.4 % Show Material materials with Mangan of 0.4 % | EN 575, DIN 1725-3 |
Nickel | 0.2 % Show Material materials with Nickel of 0.2 % | EN 575, DIN 1725-3 |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % | EN 575, DIN 1725-3 |
Titan | 4.5 - 5.5 % Show Material materials with Titan of 4.5 - 5.5 % | EN 575, DIN 1725-3 |
Vanadium | 0.3 % Show Material materials with Vanadium of 0.3 % | EN 575, DIN 1725-3 |
Zink | 0.2 % Show Material materials with Zink of 0.2 % | EN 575, DIN 1725-3 |