Chemical properties
Property | Value | Related Standards |
---|---|---|
Blei | 0.02 % Show Material materials with Blei of 0.02 % | EN 575, DIN 1725-3 |
Bor | 0.01 % Show Material materials with Bor of 0.01 % | EN 575, DIN 1725-3 |
Chrom | 0.05 % Show Material materials with Chrom of 0.05 % | EN 575, DIN 1725-3 |
Eisen | 0.3 % Show Material materials with Eisen of 0.3 % | EN 575, DIN 1725-3 |
0.30 % Show Material materials with Eisen of 0.30 % | EN 575 | |
Nickel | 0.05 % Show Material materials with Nickel of 0.05 % | EN 575, DIN 1725-3 |
Silizium | 0.3 % Show Material materials with Silizium of 0.3 % | EN 575, DIN 1725-3 |
Titan | 5.5 - 6.5 % Show Material materials with Titan of 5.5 - 6.5 % | EN 575, DIN 1725-3 |
Vanadium | 0.3 % Show Material materials with Vanadium of 0.3 % | EN 575, DIN 1725-3 |
Zink | 0.04 % Show Material materials with Zink of 0.04 % | EN 575, DIN 1725-3 |
Zinn | 0.02 % Show Material materials with Zinn of 0.02 % | EN 575, DIN 1725-3 |