Thermisch
Property | Value | Comment |
---|---|---|
Schmelzpunkt | 1480 °C Show Material materials with Schmelzpunkt of 1480 °C | Typical for Ferrovanadium |
Chemical properties
Property | Value |
---|---|
Aluminium | 2 % Show Material materials with Aluminium of 2 % |
Kohlenstoff | 0.75 % Show Material materials with Kohlenstoff of 0.75 % |
Phosphor | 0.08 % Show Material materials with Phosphor of 0.08 % |
Schwefel | 0.08 % Show Material materials with Schwefel of 0.08 % |
Silizium | 1.5 % Show Material materials with Silizium of 1.5 % |
Vanadium | 75 - 85 % Show Material materials with Vanadium of 75 - 85 % |