Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 2.65 - 2.7 g/cm³ Show Material materials with Dichte of 2.65 - 2.7 g/cm³ | Typical for Cast 3xx.x Series Aluminium |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 73 - 80 GPa Show Material materials with Elastizitätsmodul of 73 - 80 GPa | Typical for Cast 3xx.x Series Aluminium |
Poissonzahl | 23.0 °C | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Cast 3xx.x Series Aluminium |
Schubmodule | 23.0 °C | 2.8 GPa Show Material materials with Schubmodule of 2.8 GPa | Typical for Cast 3xx.x Series Aluminium |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 - 2.3E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 - 2.3E-5 1/K | Typical for Cast 3xx.x Series Aluminium |
Schmelzpunkt | 505 - 770 °C Show Material materials with Schmelzpunkt of 505 - 770 °C | Typical for Cast 3xx.x Series Aluminium | |
Spezifische Wärmekapazität | 23.0 °C | 960 - 963 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 960 - 963 J/(kg·K) | Typical for Cast 3xx.x Series Aluminium |
Wärmeleitfähigkeit | 23.0 °C | 130 - 180 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 130 - 180 W/(m·K) | Typical for Cast 3xx.x Series Aluminium |
Chemical properties
Property | Value |
---|---|
Aluminium | 82.9999 - 90.4999 % Show Material materials with Aluminium of 82.9999 - 90.4999 % |
Eisen | 0.9 % Show Material materials with Eisen of 0.9 % |
Kupfer | 2 - 4 % Show Material materials with Kupfer of 2 - 4 % |
Magnesium | 0.3 % Show Material materials with Magnesium of 0.3 % |
Mangan | 0.5 % Show Material materials with Mangan of 0.5 % |
Nickel | 0.5 % Show Material materials with Nickel of 0.5 % |
Silizium | 7.5 - 9.5 % Show Material materials with Silizium of 7.5 - 9.5 % |
Zink | 1 % Show Material materials with Zink of 1 % |
Zinn | 0.3 % Show Material materials with Zinn of 0.3 % |