Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 9.6 g/cm³ Show Material materials with Dichte of 9.6 g/cm³ | Typical for Lead Antimony |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzpunkt | 235 - 305 °C Show Material materials with Schmelzpunkt of 235 - 305 °C | Typical for Lead Antimony | |
Spezifische Wärmekapazität | 23.0 °C | 130 - 159 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 130 - 159 J/(kg·K) | Typical for Lead Antimony |
Wärmeleitfähigkeit | 23.0 °C | 24 - 34 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 24 - 34 W/(m·K) | Typical for Lead Antimony |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 % Show Material materials with Aluminium of 0.01 % |
Antimon | 14 - 15.5 % Show Material materials with Antimon of 14 - 15.5 % |
Arsen | 0.75 - 1.25 % Show Material materials with Arsen of 0.75 - 1.25 % |
Blei | 81.38 % Show Material materials with Blei of 81.38 % |
Eisen | 0.1 % Show Material materials with Eisen of 0.1 % |
Kupfer | 0.1 - 0.5 % Show Material materials with Kupfer of 0.1 - 0.5 % |
Zink | 0.05 % Show Material materials with Zink of 0.05 % |
Zinn | 0.8 - 1.2 % Show Material materials with Zinn of 0.8 - 1.2 % |