Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 2.7 g/cm³ Show Material materials with Dichte of 2.7 g/cm³ | Typical for Wrought 6000 Series Aluminium |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 70 GPa Show Material materials with Elastizitätsmodul of 70 GPa | Typical for Wrought 6000 Series Aluminium |
Plane-Strain Fracture Toughnes | 23.0 °C | 22 - 35 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22 - 35 MPa·√m | Typical for Wrought 6000 Series Aluminium |
Poissonzahl | 23.0 °C | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 6000 Series Aluminium |
Schubmodule | 23.0 °C | 26 - 26.5 GPa Show Material materials with Schubmodule of 26 - 26.5 GPa | Typical for Wrought 6000 Series Aluminium |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 - 2.4E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 - 2.4E-5 1/K | Typical for Wrought 6000 Series Aluminium |
Schmelzpunkt | 555 - 655 °C Show Material materials with Schmelzpunkt of 555 - 655 °C | Typical for Wrought 6000 Series Aluminium | |
Spezifische Wärmekapazität | 23.0 °C | 887 - 963 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 887 - 963 J/(kg·K) | Typical for Wrought 6000 Series Aluminium |
Wärmeleitfähigkeit | 23.0 °C | 170 - 220 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 170 - 220 W/(m·K) | Typical for Wrought 6000 Series Aluminium |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elektrische Leitfähigkeit | 23.0 °C | 2.10E+7 - 3.40E+7 S/m Show Material materials with Elektrische Leitfähigkeit of 2.10E+7 - 3.40E+7 S/m | Typical for Wrought 6000 Series Aluminium |
spezifischer Widerstand | 23.0 °C | 2.9E-8 - 5E-8 Ω·m Show Material materials with spezifischer Widerstand of 2.9E-8 - 5E-8 Ω·m | Typical for Wrought 6000 Series Aluminium |
Chemical properties
Property | Value |
---|---|
Aluminium | 95.8499 - 99.1999 % Show Material materials with Aluminium of 95.8499 - 99.1999 % |
Chrom | 0.3 % Show Material materials with Chrom of 0.3 % |
Eisen | 0.35 % Show Material materials with Eisen of 0.35 % |
Kupfer | 0.35 % Show Material materials with Kupfer of 0.35 % |
Magnesium | 0.4 - 0.8 % Show Material materials with Magnesium of 0.4 - 0.8 % |
Mangan | 0.5 % Show Material materials with Mangan of 0.5 % |
Silizium | 0.4 - 0.9 % Show Material materials with Silizium of 0.4 - 0.9 % |
Titan | 0.1 % Show Material materials with Titan of 0.1 % |
Zink | 0.2 % Show Material materials with Zink of 0.2 % |
Technological properties
Property | ||
---|---|---|
Workability | Excellent workability. |