Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzpunkt | 185 - 320 °C Show Material materials with Schmelzpunkt of 185 - 320 °C | Typical for Lead Tin | |
Spezifische Wärmekapazität | 23.0 °C | 213 - 239 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 213 - 239 J/(kg·K) | Typical for Lead Tin |
Wärmeleitfähigkeit | 23.0 °C | 35 - 57 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 35 - 57 W/(m·K) | Typical for Lead Tin |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 5E-3 % Show Material materials with Aluminium of 5E-3 % | |
Antimon | 2.75 % Show Material materials with Antimon of 2.75 % | |
Bismut | 0.25 % Show Material materials with Bismut of 0.25 % | |
Eisen | 0.02 % Show Material materials with Eisen of 0.02 % | |
Kupfer | 0.08 % Show Material materials with Kupfer of 0.08 % | In dipping solders, 0.5% max copper is permissible |
Zink | 5E-3 % Show Material materials with Zink of 5E-3 % | |
Zinn | 14 - 15 % Show Material materials with Zinn of 14 - 15 % |