Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.7 g/cm³ Show Material materials with Dichte of 7.7 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 20.0 °C | 169 - 183 GPa Show Material materials with Elastizitätsmodul of 169 - 183 GPa | |
Härte, Brinell | 20.0 °C | 430 - 690 [-] Show Material materials with Härte, Brinell of 430 - 690 [-] | |
Härte, Vickers | 20.0 °C | 450 - 750 [-] Show Material materials with Härte, Vickers of 450 - 750 [-] | |
Poissonzahl | 23.0 °C | 0.27 [-] Show Material materials with Poissonzahl of 0.27 [-] | Typical for Cast Iron |
Schubmodule | 23.0 °C | 41 GPa Show Material materials with Schubmodule of 41 GPa | Typical for Cast Iron |
Zugfestigkeit | 20.0 °C | 320 - 390 MPa Show Material materials with Zugfestigkeit of 320 - 390 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.5E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.5E-5 1/K | Typical for White Cast Iron |
Schmelzpunkt | 1209 °C Show Material materials with Schmelzpunkt of 1209 °C | Typical for White Cast Iron | |
Spezifische Wärmekapazität | 23.0 °C | 460 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 J/(kg·K) | Typical for White Cast Iron |
Wärmeleitfähigkeit | 20.0 °C | 14 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 14 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 20.0 °C | 8E-7 Ω·m Show Material materials with spezifischer Widerstand of 8E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Chrom | 1.4 - 2.4 % Show Material materials with Chrom of 1.4 - 2.4 % |
Kohlenstoff | 2.6 - 2.9 % Show Material materials with Kohlenstoff of 2.6 - 2.9 % |
Mangan | 0.3 - 0.7 % Show Material materials with Mangan of 0.3 - 0.7 % |
Molybdän | 0.5 % Show Material materials with Molybdän of 0.5 % |
Nickel | 3.3 - 5 % Show Material materials with Nickel of 3.3 - 5 % |
Silizium | 0.2 - 0.8 % Show Material materials with Silizium of 0.2 - 0.8 % |