Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.7 g/cm³ Show Material materials with Dichte of 7.7 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 20.0 °C | 154 - 190 GPa Show Material materials with Elastizitätsmodul of 154 - 190 GPa | |
Härte, Vickers | 20.0 °C | 400 [-] Show Material materials with Härte, Vickers of 400 [-] | |
Poissonzahl | 23.0 °C | 0.27 [-] Show Material materials with Poissonzahl of 0.27 [-] | Typical for Cast Iron |
Schubmodule | 23.0 °C | 41 GPa Show Material materials with Schubmodule of 41 GPa | Typical for Cast Iron |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.5E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.5E-5 1/K | Typical for White Cast Iron |
Schmelzpunkt | 1209 °C Show Material materials with Schmelzpunkt of 1209 °C | Typical for White Cast Iron | |
Spezifische Wärmekapazität | 23.0 °C | 460 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 J/(kg·K) | Typical for White Cast Iron |
Wärmeleitfähigkeit | 20.0 °C | 13.8 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 13.8 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Chrom | 14 - 17 % Show Material materials with Chrom of 14 - 17 % |
Kohlenstoff | 2.3 - 3.6 % Show Material materials with Kohlenstoff of 2.3 - 3.6 % |
Mangan | 0.5 - 1 % Show Material materials with Mangan of 0.5 - 1 % |
Molybdän | 1 - 3 % Show Material materials with Molybdän of 1 - 3 % |
Nickel | 0.7 % Show Material materials with Nickel of 0.7 % |
Silizium | 0.2 - 0.8 % Show Material materials with Silizium of 0.2 - 0.8 % |