Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.3 g/cm³ Show Material materials with Dichte of 8.3 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 12 % Show Material materials with Dehnung of 12 % |
Elastizitätsmodul | 20.0 °C | 152 GPa Show Material materials with Elastizitätsmodul of 152 GPa |
Härte, Brinell | 20.0 °C | 80 [-] Show Material materials with Härte, Brinell of 80 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 120 MPa Show Material materials with Streckgrenze Rp 0,2 of 120 MPa |
Zugfestigkeit | 20.0 °C | 320 MPa Show Material materials with Zugfestigkeit of 320 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 8.5E-6 - 1.4E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 8.5E-6 - 1.4E-5 1/K | Typical for Pure/Low Nickel Alloy |
Schmelzpunkt | 1400 - 1500 °C Show Material materials with Schmelzpunkt of 1400 - 1500 °C | Typical for Pure/Low Nickel Alloy | |
Spezifische Wärmekapazität | 23.0 °C | 430 - 532 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 430 - 532 J/(kg·K) | Typical for Pure/Low Nickel Alloy |
Wärmeleitfähigkeit | 23.0 °C | 18 - 86 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 18 - 86 W/(m·K) | Typical for Pure/Low Nickel Alloy |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 20.0 °C | 2.85E-7 Ω·m Show Material materials with spezifischer Widerstand of 2.85E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Eisen | 1 % Show Material materials with Eisen of 1 % |
Kohlenstoff | 1 % Show Material materials with Kohlenstoff of 1 % |
Kupfer | 1.2 % Show Material materials with Kupfer of 1.2 % |
Mangan | 1.5 % Show Material materials with Mangan of 1.5 % |
Nickel | 95 % Show Material materials with Nickel of 95 % |
Silizium | 2 % Show Material materials with Silizium of 2 % |
Technological properties
Property | ||
---|---|---|
Processing methods | sand casting, separately cast test sample |