Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.2 g/cm³ Show Material materials with Dichte of 8.2 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 25 % Show Material materials with Dehnung of 25 % |
Elastizitätsmodul | 20.0 °C | 200 GPa Show Material materials with Elastizitätsmodul of 200 GPa |
Härte, Brinell | 20.0 °C | 230 [-] Show Material materials with Härte, Brinell of 230 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 220 MPa Show Material materials with Streckgrenze Rp 0,2 of 220 MPa |
Streckgrenze Rp 1,0 | 20.0 °C | 250 MPa Show Material materials with Streckgrenze Rp 1,0 of 250 MPa |
Zugfestigkeit | 20.0 °C | 600 MPa Show Material materials with Zugfestigkeit of 600 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 1.35E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.35E-5 1/K | |
200.0 °C | 1.4E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.4E-5 1/K | ||
400.0 °C | 1.5E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.5E-5 1/K | ||
600.0 °C | 1.55E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.55E-5 1/K | ||
800.0 °C | 1.6E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 1/K | ||
Max. Betriebstemperatur, lang | 0 - 1150 °C Show Material materials with Max. Betriebstemperatur, lang of 0 - 1150 °C | ||
Schmelzpunkt | 1400 °C Show Material materials with Schmelzpunkt of 1400 °C | Typical for Nickel Chromium Alloy | |
Spezifische Wärmekapazität | 20.0 °C | 460 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 J/(kg·K) | |
Wärmeleitfähigkeit | 20.0 °C | 13 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 13 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 20.0 °C | 1.1E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.1E-6 Ω·m |
100.0 °C | 1.14E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.14E-6 Ω·m | |
200.0 °C | 1.16E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.16E-6 Ω·m | |
300.0 °C | 1.18E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.18E-6 Ω·m | |
400.0 °C | 1.2E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.2E-6 Ω·m | |
500.0 °C | 1.22E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.22E-6 Ω·m | |
600.0 °C | 1.21E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.21E-6 Ω·m | |
700.0 °C | 1.21E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.21E-6 Ω·m | |
800.0 °C | 1.22E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.22E-6 Ω·m | |
900.0 °C | 1.23E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.23E-6 Ω·m | |
1000.0 °C | 1.24E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.24E-6 Ω·m | |
1100.0 °C | 1.26E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.26E-6 Ω·m | |
1200.0 °C | 1.28E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.28E-6 Ω·m | |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.3 % Show Material materials with Aluminium of 0.3 % |
Chrom | 19 - 21 % Show Material materials with Chrom of 19 - 21 % |
Eisen | 1 % Show Material materials with Eisen of 1 % |
Kohlenstoff | 0.15 % Show Material materials with Kohlenstoff of 0.15 % |
Kupfer | 0.5 % Show Material materials with Kupfer of 0.5 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Nickel | 75 % Show Material materials with Nickel of 75 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.5 - 2 % Show Material materials with Silizium of 0.5 - 2 % |