Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.7 - 8.7 g/cm³ Show Material materials with Dichte of 7.7 - 8.7 g/cm³ | Typical for Leaded Phosphor Bronze |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 10 % Show Material materials with Dehnung A50 of 10 % | |
Elastizitätsmodul | 23.0 °C | 110 - 130 GPa Show Material materials with Elastizitätsmodul of 110 - 130 GPa | Typical for Leaded Phosphor Bronze |
Poissonzahl | 23.0 °C | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Leaded Phosphor Bronze |
Streckgrenze Rp0,5 | 23.0 °C | 310 MPa Show Material materials with Streckgrenze Rp0,5 of 310 MPa | |
Zugfestigkeit | 23.0 °C | 655 MPa Show Material materials with Zugfestigkeit of 655 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.5E-5 - 1.9E-5 1/K | Typical for Leaded Phosphor Bronze |
Spezifische Wärmekapazität | 23.0 °C | 380 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 380 J/(kg·K) | Typical for Leaded Phosphor Bronze |
Chemical properties
Property | Value |
---|---|
Aluminium | 10 - 11.5 % Show Material materials with Aluminium of 10 - 11.5 % |
Eisen | 2 - 4.5 % Show Material materials with Eisen of 2 - 4.5 % |
Mangan | 0.3 % Show Material materials with Mangan of 0.3 % |
Silizium | 0.25 % Show Material materials with Silizium of 0.25 % |
Zinn | 0.2 % Show Material materials with Zinn of 0.2 % |