Chemical properties
Property | Value |
---|---|
Aluminium | 9 - 11 % Show Material materials with Aluminium of 9 - 11 % |
Eisen | 2 - 4 % Show Material materials with Eisen of 2 - 4 % |
Mangan | 1.5 % Show Material materials with Mangan of 1.5 % |
Nickel | 4 - 5.5 % Show Material materials with Nickel of 4 - 5.5 % |
Silizium | 0.25 % Show Material materials with Silizium of 0.25 % |
Zink | 0.3 % Show Material materials with Zink of 0.3 % |
Zinn | 0.2 % Show Material materials with Zinn of 0.2 % |