Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 15 % Show Material materials with Dehnung A50 of 15 % |
Streckgrenze Rp0,5 | 20.0 °C | 275 - 345 MPa Show Material materials with Streckgrenze Rp0,5 of 275 - 345 MPa |
Zugfestigkeit | 20.0 °C | 620 MPa Show Material materials with Zugfestigkeit of 620 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 8.7 - 9.5 % Show Material materials with Aluminium of 8.7 - 9.5 % |
Blei | 0.02 % Show Material materials with Blei of 0.02 % |
Eisen | 3.5 - 4.3 % Show Material materials with Eisen of 3.5 - 4.3 % |
Mangan | 1.2 - 2 % Show Material materials with Mangan of 1.2 - 2 % |
Nickel | 4 - 4.8 % Show Material materials with Nickel of 4 - 4.8 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |